Surface fuzzing. The case and bag webbing surface fuzzing and needle edge defects often occur in the production process. What are the reasons and how to solve or prevent them? The following manufacturer's knitting will tell you. Causes of surface fuzzing of luggage webbing: needle edge fuzzing, cloth edge fuzzing. Precautions: The needle plate has been used for a long time and has been damaged. Replace the needle plate with a new one; The knitting needle has been damaged and replaced with a new one; The pressure plate is pressed too tightly, and loosen the pressure plate; If the weft is not hung completely, adjust the distance between the weft needle and the knitting needle so that the weft can be hung completely. The steel buckle of the weft yarn is hung, and the weft yarn is put into the weft rod; If the steel buckle is damaged, replace it with another one; The raw material itself is hairy. If it is partly hairy, replace it. If it is too hairy, make a full inspection belt after finishing the goods.

Moisture in the air may cause special Clothing ribbon When the webbing contacts with the passengers' clothes, the spots and colors on the luggage webbing will also be transferred to the clothes, so Changchun Clothing ribbon It shall have anti spot fading property, which is also called spot color fastness. The spot color fastness test includes multi fiber test and filter paper test. The multi fiber test is to clamp a sample of tissue belt between two layers of colored cloth. Clamp Clothing ribbon Immerse the cloth with distilled water and completely wet it. Then squeeze the water out of the extruder, and then clamp these colored cloth wrapped with selvedge webbing into the plexiglass sheet, put it into the sample holder, and lock the sample holder. This rack is placed in a high and low temperature box at a certain temperature, and after reaching the specified time. Take out the sample and hang the colored cloth.

Causes of bleeding. Some customers will customize the printing, but the PP fabric manufacturers sometimes have color bleeding when printing the PP ribbon, so the manufacturers should pay attention to the reasons when printing. Only by understanding these reasons can we reduce the occurrence of various conditions in the future use. What are the reasons for color bleeding when printing? There is dirt on the surface of the machine during printing. Cleaning up during production can reduce these problems.

Flat screen printing. The printing mould is a polyester or nylon screen (pattern) fixed on a square frame with hollow patterns. The pattern on the pattern plate can pass through the color paste, and the mesh without pattern can be sealed with a polymer film. When printing, the pattern is pressed against the fabric, and the color paste is placed on the pattern. The scraper is used to repeatedly scrape and press the color paste to reach the fabric surface through the pattern. Flat screen printing has low production efficiency, but wide adaptability and flexible application, suitable for small batch and multi variety production. Water slurry printing of bag webbing.

At present, more than 90% of the market is made of cotton polyester thread or polyester cotton thread, but there are few pure cotton threads in the market, and the price is surprisingly high! Polyester cotton yarn just neutralizes the advantages of pure cotton and polyester, depending on the composition of polyester in cotton. Generally, the yarn of cotton ribbon is made by adding a small amount of polyester into cotton, so that it can have the advantages of pure cotton and polyester cotton. It is easy to wash, heat resistant, alkali resistant, moisturizing, sanitary, wear-resistant, not shrink, not easy to wrinkle, not easy to deform, not easy to stick wool, and so on! The key is that the proportion of cotton and polyester is appropriate! The identification method of pure cotton webbing and polyester cotton webbing is simply to take the cut thread and burn it. If there is any hard block, it is polyester cotton yarn containing polyester, and if it is completely reduced to ashes, it is authentic pure cotton.