Dalian special Braided rope Flat screen printing. The printing mould is a polyester or nylon screen (pattern) fixed on a square frame with hollow patterns. The pattern on the pattern plate can pass through the color paste, and the mesh without pattern can be sealed with a polymer film. When printing, the pattern is pressed against the fabric, and the color paste is placed on the pattern. The scraper is used to repeatedly scrape and press the color paste to reach the fabric surface through the pattern. special Braided rope Flat screen printing has low production efficiency, but wide adaptability and flexible application, suitable for small batch and multi variety production. Water slurry printing of bag webbing.

Hygiene: It is a natural fiber, and its main component is cellulose, with a small amount of waxy substances, nitrogen and pectin. After various inspections and practices, the pure cotton ribbon has no stimulation or negative effect when contacting with the skin. It is beneficial to the human body and has good sanitary performance after being worn for a long time. Heat resistance: the heat resistance is good. When the temperature is below 110 ℃, it will only cause water evaporation on the webbing and will not damage the fiber. Therefore, the use, washing, printing and dyeing of pure cotton webbing at room temperature have no impact on the webbing, which improves the washing and wear resistance of pure cotton edging webbing.

The progress of process technology has brought about the upgrading of edging webbing products. In 1979, the trial production of the domestic generation SD9-9 rubber ingot belt was successful, which ended the history of rubber ingot belt products relying on imports. After the weft tube is formed by the yarn warp cylinder and weft winding, it is inserted on the fixed gear seat of the knitting machine, and the weft tube rotates along the 8-shaped track to draw the yarns to cross weave with each other. Usually, the number of spindles is even, the woven tape is tubular, the number of spindles is odd, and the woven tape is flat. Spindle weaving technology has been applied since old China. The number of spindles varies from 9 to 100 due to different equipment.

After the weft tube is formed by the yarn warp cylinder and weft winding, it is inserted on the fixed gear seat of the knitting machine, and the weft tube rotates along the 8-shaped track to draw the yarns to cross weave with each other. Usually, the number of spindles is even, the woven tape is tubular, the number of spindles is odd, and the woven tape is flat. Spindle weaving technology has been applied since old China. The number of spindles varies from 9 to 100 due to different equipment. The basic process of weaving is: bleaching and dyeing - weft rolling - weaving - off machine shearing - packaging. Since 1960, many technical innovations have been carried out on the knitting machine, mainly including the enlargement of peach plate diameter, the installation of an automatic stop device for breaking rubber bands, and the replacement of iron ingots with nylon ingots. The improvement of these equipment has increased the vehicle speed to 160~190 rpm, doubled the stand rate and greatly improved the product quality.

Surface fuzzing. The case and bag webbing surface fuzzing and needle edge defects often occur in the production process. What are the reasons and how to solve or prevent them? The following manufacturer's knitting will tell you. Causes of surface fuzzing of luggage webbing: needle edge fuzzing, cloth edge fuzzing. Precautions: The needle plate has been used for a long time and has been damaged. Replace the needle plate with a new one; The knitting needle has been damaged and replaced with a new one; The pressure plate is pressed too tightly, and loosen the pressure plate; If the weft is not hung completely, adjust the distance between the weft needle and the knitting needle so that the weft can be hung completely. The steel buckle of the weft yarn is hung, and the weft yarn is put into the weft rod; If the steel buckle is damaged, replace it with another one; The raw material itself is hairy. If it is partly hairy, replace it. If it is too hairy, make a full inspection belt after finishing the goods.